An Exacting Process

The process of lnequering is on "nite patiencs Soned wood is the usual foundation.

This is planned and polished, and when every flaw has been removed a piece of silk gauze or fine paper is pasted on. The surface thus prepared is next covered with a. pre-aration which varies; of burnt clay mixed with varnish, or of red Istone ground fine and blended gall. When this is dry it is smoothed with a whetstone and rubbed with wax. On this groun work the lacquer is laid very eventy thin coats with a hard flat brush. he number of coats varies accord-to the quality of the work; the rule is "Never fewer than three, never more than 18." Each coat dried before the next is laid on, and will not harden properly except in an atmosphere that is slightly damp, warm and humid. It is then polished and another coat of lacquer applied, and the drying, polishing, and lay: ing on are repeated until the proper: depth has been achieved and the: glossy, lustrous and almost metallic surface is ready for decoration.

Text read from the printed page and cleaned; old type leaves the occasional error.

Your account